镁碳砖|
品名 指标 |
MgO%≥ |
C≤ |
显气孔率A.P%≤ |
常温耐压强度Mpa≥ |
体密B.Dg/m3≥ |
0.2Mpa荷软开始温度≥℃ |
|
DN-10B |
72 |
10 |
6 |
30 |
2.8 |
1700 |
|
DN-10A |
74 |
10 |
4 |
35 |
2.8 |
1700 |
|
DN-14B |
70 |
14 |
7 |
25 |
2.9 |
1750 |
|
DN-14A |
72 |
14 |
5 |
30 |
2.9 |
1750 |
|
DN-18B |
68 |
18 |
7 |
25 |
3 |
1750 |
|
DN-18A |
70 |
18 |
5 |
28 |
3 |
1750 |
铝镁碳砖|
品名 指标 |
MgO%≥ |
AI2O3% |
C≤ |
显气孔率A.P%≤ |
常温耐压强度Mpa≥ |
0.2Mpa荷软开始温度≥℃ |
|
DN-50 |
5-10 |
50 |
5 |
18 |
20 |
1350 |
|
DN-55 |
5-10 |
55 |
5 |
10 |
20 |
1580 |
|
DN-60 |
12 |
60 |
8 |
8 |
20 |
1610 |
镁碳砖|
品名 指标 |
MgO%≥ |
C≤ |
显气孔率A.P%≤ |
常温耐压强度Mpa≥ |
体密B.Dg/m3≥ |
0.2Mpa荷软开始温度≥℃ |
|
DN-10B |
72 |
10 |
6 |
30 |
2.8 |
1700 |
|
DN-10A |
74 |
10 |
4 |
35 |
2.8 |
1700 |
|
DN-14B |
70 |
14 |
7 |
25 |
2.9 |
1750 |
|
DN-14A |
72 |
14 |
5 |
30 |
2.9 |
1750 |
|
DN-18B |
68 |
18 |
7 |
25 |
3 |
1750 |
|
DN-18A |
70 |
18 |
5 |
28 |
3 |
1750 |
铝镁碳砖|
品名 指标 |
MgO%≥ |
AI2O3% |
C≤ |
显气孔率A.P%≤ |
常温耐压强度Mpa≥ |
0.2Mpa荷软开始温度≥℃ |
|
DN-50 |
5-10 |
50 |
5 |
18 |
20 |
1350 |
|
DN-55 |
5-10 |
55 |
5 |
10 |
20 |
1580 |
|
DN-60 |
12 |
60 |
8 |
8 |
20 |
1610 |